1. Resin Viscosity gets higher, and will this affect the printing?
Exploding in UV or sunlight; ambient temperature becomes low; or stock resin in a room the air conditioner working. All these will lead to viscosity become higher. Please store and print between 20-30 degrees C.
2. There are white residue on resin models after post curing
The resin residues are not cleaned well.
The alcohol purity is not enough or cleaned by water. Please clean resin model by ≥95% alcohol and make sure the residue are cleaned.
Please dry up resin models with lint free wiper or hair conditioner.
3. Resin models get soft and distortion
Cleaning time is too long. We suggest cleaning with ≥95% alcohol within 60s.
Please dry the resin model and post cuing by UV chamber or sunlight.
sure every side of the model is cured until model is dry and strong enough.
4. There are breaks or holes on resin models at same XY axis position.
First, check if there are on the release film or LCD screen. If no, please check the LCD screen.
5. Obvious layer mark on resin models.
Defective Z axis lead screw or the screw is loose.
6. stocked small holes , bad details, no sharp angles, the print is bigger than 3d model.
The cuing time is too long. Shorten curing time for each layer.
Notice:
Water washable 3d printing resin is cleaned by water.